dc.description.abstract | The study of chitosan polymer behavior as a solid thin film electrolytes have attracted many researchers to involves into the conductivity exploration of chitosan polymer electrolytes. The prepared chitosan acetate doped glycolic acid (CA-GA) thin film was done in order to find the highest ionic conductivity of chitosan doped glycolic acid at different glycolic acid (GA) concentration and temperature. These thin films doped GA was made by using solution cast technique and analyzed by Fourier Transform Infrared Spectroscopy (FTIR) and Electrochemical Impedence Spectroscopy (EIS). FTIR analysis shows that the carbonyl (C=NHR) in pure chitosan (CS) spectrum has been shifted to 1637 cm ·1in the pure CA. The band at 900 cm· | en_US |
dc.language.iso | en | en_US |
dc.publisher | Universiti Malaysia Terengganu | en_US |
dc.subject | Santana Dee Colone Jani | en_US |
dc.subject | LP 27 FST 3 2008 | en_US |
dc.title | Electrical and ftir study of chitosan based polymer electrolytes doped glycolic acid | en_US |
dc.type | Working Paper | en_US |
Appears in Collections: | Fakulti Sains dan Teknologi |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
LP 27 FST 3 2008 Abstract.pdf | 564.87 kB | Adobe PDF | View/Open | |
LP 27 FST 3 2008 Full text.pdf Restricted Access | 3.4 MB | Adobe PDF | View/Open Request a copy |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.